The basic information
Chemical composition |
LiNbO3 |
Melting point |
1250℃ |
The density |
4.6g/cm3 |
Common direction |
Y128°、Y41°、Y64°、Y、X、Z and so on |
Curie temperature |
1136-1144℃ |
Hardness (mo) |
5 |
Surface acoustic performance
Cutting direction |
Direction of propagation |
Surface wave velocity |
The coupling coefficient(%) |
Temperature coefficient of delay(ppm/℃) |
128°Y-Cut |
X-Axis |
3980 |
5.5 |
75 |
64°Y-Cut |
X-Axis |
4742 |
11.2 |
70 |
41°Y-Cut |
X-Axis |
4792 |
17.3 |
50 |
Y-Cut |
X-Axis |
3488 |
4.9 |
94 |